dc.contributor.authorOliveira, Joselito Bonifáciopt_BR
dc.contributor.authorVale, Ailton T.pt_BR
dc.contributor.authorMelo, José Teodoro dept_BR
dc.date.accessioned2017-12-07T04:45:58Z-
dc.date.available2017-12-07T04:45:58Z-
dc.date.issued2006pt_BR
dc.identifier.citationCiênc. Florest.,v.16,n.1,p.89-97,2006pt_BR
dc.identifier.urihttp://repositorio.unb.br/handle/10482/26813-
dc.description.abstractRESUMO O objetivo do presente trabalho foi caracterizar a madeira de Sclerolobium paniculatum Vogel, de 18 anos de idade, oriunda de plantio homogêneo sob diferentes níveis de adubação localizado na Embrapa- Cerrados, DF, quanto à contração e às características mecânicas (flexão estática, compressão paralela às fibras e cisalhamento). Não foram encontradas diferenças significativas entre as médias das variáveis estudadas que apresentaram os seguintes valores: resistência máxima à flexão estática (ƒb = 650kg/cm2), módulo de elasticidade (E = 59.877kg/cm2), resistência máxima à compressão axial (ƒc = 296kg/cm2) e resistência máxima ao cisalhamento (ƒν = 131kg/cm2). Para cisalhamento e compressão axial, a testemunha apresentou o maior valor absoluto para MOR. A madeira de Sclerolobium paniculatum apresentou um elevado número de galhos, implicando uma elevada quantidade de nós. Os tratos culturais em plantios homogêneos de Sclerolobium paniculatum devem prever a retirada de galhos para produzir madeira de qualidade superior.pt_BR
dc.description.abstractABSTRACT The purposa of this work was to study the influence of fertilization on wood quality of Sclerolobium paniculatum Vogel. A homogeneous planting trial, under different levels of liming and phosphorus, was established by Embrapa-Cerrados 18 years ago in Planaltina, Distrito Federal, Brazil, tropical wood savanna region. Mechanical tests conducted were static bending, parallel compression to grain, shear strength and shrinkage. No significant differences were observed for mechanical properties or for shrinkage, which presented: ƒb = 650kg/cm2, E = 59.877kg/cm2, ƒc = 296kg/cm2 e ƒν = 131kg/cm2. Control treatment showed highest values for shear strength and compression parallel to grain. Too many branches in all trees and also too many knots in lumber were observed. Pruning is recommended for homogeneous planting of Sclerolobium paniculatum to avoid knots in order to be produced wood of superior quality.pt_BR
dc.language.isoporpt_BR
dc.publisherUniversidade Federal de Santa Mariapt_BR
dc.rightsAcesso Abertopt_BR
dc.titleCARACTERIZAÇÃO MECÂNICA E CONTRAÇÃO DA MADEIRA DE Sclerolobium paniculatum Vogel CULTIVADO EM UM PLANTIO HOMOGÊNEO SOB DIFERENTES NÍVEIS DE ADUBAÇÃOpt_BR
dc.titleMECHANICAL CHARACTERIZATION AND SHRINKAGE OF Sclerolobium paniculatum Vogel WOOD IN A HOMOGENEOUS PLANTING UNDER DIFFERENT LEVELS OF FERTILIZATIONpt_BR
dc.typeArtigopt_BR
dc.subject.keywordCaracterizaçãopt_BR
dc.subject.keywordMadeirapt_BR
dc.subject.keywordSlerolobium paniculatumpt_BR
dc.identifier.doihttps://dx.doi.org/10.5902/198050981890pt_BR
dc.description.unidadeEm processamento-
Appears in Collections:Artigos publicados em periódicos e afins

Show simple item record " class="statisticsLink btn btn-primary" href="/handle/10482/26813/statistics">



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.